On Press Issue: Chalking

Potential Causes

Ink film is too thin because ink strength is too strong

Solution: Reformulate ink or make weaker at press by adding extender or tint base.

Fountain solution pH too low

Solution: Check pH of solution. pH of lower than 3.5 can slow drying. Adjust pH of fountain solution. 

Ink body is too soft causing excess penetration into substrate

Solution: Reformulate ink for heavier body showing penetration. Heavy body, high solid varnishes added at press will help.